Corrosion: Materials
Corrosion of Intermetallics
-
Published:2005
Abstract
This article reviews the corrosion behavior of intermetallics for the modeling of the corrosion processes and for devising a strategy to create corrosion protective systems through alloy and coating design. It discusses the high-temperature corrosion properties of intermetallics and aqueous corrosion properties. Thermodynamic principles in the context of high-temperature corrosion and information on oxidation; sulfidation; hot corrosion of NiAl-, FeAl-, and TiAl-based intermetallics; and silicides are included. The article explores the thermodynamic consideration, ordering influencing kinetics, stress-cracking corrosion, and hydrogen embrittlement of aqueous corrosion. It also explains the practical issues dealing with the corrosion problems.
Sign in
ASM members
Member Sign InP.K. Datta, H.L. Du, J.S. Burnell-Gray, R.E. Ricker, Corrosion of Intermetallics, Corrosion: Materials, Vol 13B, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2005, p 490–512, https://doi.org/10.31399/asm.hb.v13b.a0003837
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.