Abstract

Nonferrous metals and alloys are widely used to resist corrosion. This article describes the most widely used nonferrous metals, such as aluminum, copper, nickel, and titanium. It also provides information on several specialty nonferrous products that cannot easily be categorized by elemental base.

You do not currently have access to this chapter.
Don't already have an account? Register

Paul Crook, Introduction to Corrosion of Nonferrous Metals and Specialty Products, Corrosion: Materials, Vol 13B, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2005, p 93–94, https://doi.org/10.31399/asm.hb.v13b.a0003814