Weathering steels contain deliberate additions of alloying elements intended to increase the atmospheric corrosion resistance of steel. This article provides an overview of atmospheric corrosion testing. It describes the estimation of the atmospheric corrosion behavior of weathering steels by two methods such as short-term exposure tests and calculation of a corrosion index based on the steel composition. The article highlights some generalities about corrosion mechanisms. Based on the mechanism of atmospheric corrosion resistance of weathering steel, working rules for creating the protective oxide film have evolved. The article also provides case histories that illustrate both the violations of these...