Abstract

Natural and synthetic rubber linings are used extensively in many industries for their corrosion and/or abrasion resistance. These industries include transportation, chemical processing, water treatment, power, mineral processing, and mining. This article provides information on soft natural rubber, semihard natural rubber, hard natural rubber, neoprene or polychloroprene, chlorobutyl, three-ply linings, nitrile, and ethylene propylene with a diene monomer. Emphasis is placed on advantages, disadvantages, and common uses of each material discussed.