This article reviews various test methods used for evaluating the corrosion resistance of powder metallurgy stainless steels. These include immersion testing, salt spray testing, and electrochemical testing. The article discusses the factors that affect corrosion resistance of sintered stainless steels: compaction-related factors, sintering-related factors, and effects of alloy composition. Corrosion resistance data for sintered stainless steels is provided.