Abstract

This article focuses on mechanical testing characterization of blended elemental powder metallurgy (PM) titanium alloys and prealloyed PM titanium alloys. It examines the tensile properties, fracture toughness, stress-corrosion threshold resistance, fatigue strength, crack propagation properties, and processing-microstructure-property relationships of these alloys. The article also reviews five considerations for powder process selection.