This article provides a summary of the conventional technologies used for titanium powder production. It focuses on the various processes for titanium powder production, namely, Hunter, Kroll, Armstrong, MER, TIRO, FFC-Cambridge, Chinuka, and CSIR processes. Employment of titanium powder significantly improves the synthesis of titanium and its alloys.