Stainless steels are highly alloyed materials in comparison to most other popular powder metallurgy (PM) materials, such as low-alloy steels, copper alloys, and aluminum alloys. This article provides an overview of the history of PM stainless steels.

Abstract

Stainless steels are primarily alloys of iron and chromium. They are grouped into five families, primarily based on their microstructure: ferritic, austenitic, martensitic, duplex, and precipitation hardening. Three out of the five families of stainless steels, namely, austenitic, ferritic, and martensitic, are well suited for manufacture via conventional powder metallurgy (PM) processes. This article presents the iron-chromium partial phase diagram to illustrate the changes in the temperature range when pure iron is alloyed with chromium. It describes AISI and UNS numbering systems, which are used as an identification system for stainless steels. The article tabulates the material designations of stainless steels in accordance with the Metal Powder Industries Federation. It also details the characteristics and chemical composition of wrought and PM stainless steels.

You do not currently have access to this chapter.
Don't already have an account? Register

2015. "Powder Metallurgy Stainless Steels", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal