Abstract

This article discusses the requirements for safe design, installation, operation, inspection, testing, and maintenance of sintering atmosphere generators and atmosphere supply systems for both personal and environment safety. The four intrinsic dangers associated with producing and using common sintering atmosphere gases are explosion, fire, toxicity, and asphyxiation.

You do not currently have access to this chapter.
Don't already have an account? Register

Thomas Philips, Harb Nayar, Safety and Environmental Concerns in Using Sintering Atmospheres, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 247–250, https://doi.org/10.31399/asm.hb.v07.a0006137