This article describes several factors, which help in determining the compressibility of metal powders: particle shape, density, composition, hardness, particle size, lubrication, and compacting. It discusses the uses of annealing metal powders and describes compressibility testing of the powders. The article details green strength and its mechanism and the variables affecting the strength. It also discusses two test methods for determining the green strength: the Rattler test and the transverse bend test.

Abstract

This article discusses continuum modeling, which is the most relevant approach in modeling grain growth, densification, and deformation during sintering. Continuum plasticity models are frequently used to describe the mechanical response of metal powders during compaction. The article illustrates the typical procedure for computer simulation for press and sinter process. It describes the procedure to obtain the material properties based on the generalized Shima-Oyane model. The article presents a wide variety of tests, accounting for data on the grain growth, densification, and distortion where these data help in the development of a constitutive model for sintering simulation. Finally, the article provides information on the simulation approaches used to optimize die compaction and sintering.

You do not currently have access to this chapter.
Don't already have an account? Register

Metal Powder Compaction, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal