Abstract

Commercial zinc plating is accomplished by a number of distinctively different systems: cyanide baths, alkaline noncyanide baths, and acid chloride baths. This article focuses on the composition, advantages, disadvantages, operating parameters, and applications of each of the baths. It provides information on the control of thicknesses of zinc specified for service in various indoor and outdoor atmospheres and on the similarities between cadmium and zinc plating.

You do not currently have access to this chapter.
Don't already have an account? Register

A. Sato, 1994. "Zinc Plating", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.