Wipe solvents are used to remove contaminants from a workpiece before it undergoes manufacturing operations that require clean surfaces, such as bonding, sealing, painting, welding, plating, specialized surface treatment procedures, and others. This article describes the evaluation parameters for wipe solvent cleaners, including methyl ethyl ketone, methyl isobutyl ketone, trichloroethene, tetrachloroethylene, acetone, toluene, dichloromethane, benzene, xylene, and other alternate wipe solvent cleaners. It contains a table that lists the compositions and properties of wipe solvent cleaners.

You do not currently have access to this chapter.
Don't already have an account? Register

Mark T. Carroll, 1994. "Compliant Wipe Solvent Cleaners", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.