Mechanical plating is a method for coating ferrous metals, copper alloys, lead, stainless steel, and certain types of castings by tumbling the parts in a mixture of glass beads, metallic dust or powder, promoter or accelerator chemicals, and water. It offers a straightforward alternative method for achieving desired mechanical and galvanic properties with an extremely low risk of hydrogen embrittlement. This article provides a detailed description of the equipment, process steps, process capabilities, applicable parts, specific characteristics, advantages, limitations, post treatments, and waste treatment of mechanical plating.