A catalyst must be designed to have high activity and selectivity. The chemical process being catalyzed should have high productivity within a specified reactor volume with high reaction rates for the desired reactions and low rates for undesired reaction pathways. This article reviews the most general catalyst preparation procedures: impregnation, ion exchange, and precipitation. It explains the various categorizations of carrier materials: active carriers such as alumina, silica-alumina, zeolites, titanium oxide, and carbon in powder or particulate form; inert carriers such as silica, in powder or particulate form; and structural supports such as the monoliths upon which catalyzed carders are deposited. The article also describes catalyst powder processing techniques for tableting, beading, extrusion, spray drying and honeycombing.

You do not currently have access to this chapter.
Don't already have an account? Register

Michel Deeba, Jennifer S. Feeley, 1994. "Surface Engineering for Chemical Activity", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal