Abstract

Standardization, repeatability, convenience, short testing time, and simple measuring and ranking techniques are desirable in wear and erosion tests. This article provides a brief review of the wear testing methods and wear and erosion test equipment. General elements of a wear test, namely, simulation, acceleration, specimen preparation, control, measurement, and reporting, are reviewed.