This article focuses on the influence of various work material properties, namely, hardness; toughness; stiffness; ductility; thermal, electrical, and magnetic properties; and microstructure effects on finishing methods. It also addresses the relative response of work materials, such as metals, ceramics, and composites, to grinding.