Abstract

Painting is a generic term for the application of a thin organic coating to the surface of a material for decorative, protective, or functional purposes. This article provides a detailed account of the types and selection factors of paints and the various application methods, including conventional air atomized, airless, and electrostatic spray; roller coating; dip coating; flow coating; curtain coating; tumble coating; electrocoating; and powder coating. Surface preparation methods and prepaint treatments for coating systems are also discussed. The article includes information on quality control procedures, causes of paint film defects, cost calculation, and safety and environmental precautions. The composition and characteristics of organic coatings, coating system selection factors, the types of paints for structural steel, and the applications of paint on structural steel are also reviewed.

You do not currently have access to this chapter.
Don't already have an account? Register
Close Modal

or Create an Account

Close Modal
Close Modal