Surface Engineering
Rust-Preventive Compounds
-
Published:1994
Abstract
Rust-preventive compounds are removable coatings used for the protection of the surfaces of iron, steel, coated or galvanized products, and other alloys. This article describes the basic parts of rust-preventive compounds, namely, carrier, film former, polar materials, and specialty additives. It explains types of rust-preventive compounds, including dry films and water-based dry films. The article also discusses the methods of application of various compounds, such as petrolatum compounds and emulsion compounds. It contains tables that provide information on the characteristics, applications, and physical properties of rust-preventive materials covered by military specifications. Finally, the article describes the various considerations and parameters for selecting rust-preventive materials.
Sign in
ASM members
Member Sign InHarry D. Ferrier, Jr., Rust-Preventive Compounds, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 412–420, https://doi.org/10.31399/asm.hb.v05.a0001276
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.