Abstract

Electrodeposits of cadmium are used to protect steel and cast iron against corrosion. This article provides an overview of the surface preparation of, and brighteners used in, cyanide baths. It focuses on the anode system, current density, deposition rates, and bath temperature of cadmium plating with attention to the materials of construction and equipment used. The article provides a description of the selection of plating method with examples, applications, and several postplating processes of cadmium plating.