The electroplating of platinum-group metals (PGMs) from aqueous electrolytes for engineering applications is limited principally to palladium and, to a lesser extent, to platinum, rhodium, and thin layers of ruthenium. This article provides a discussion on the plating operations of these PGMs along with the types of anodes used in the process.