This article focuses on the influence of various work material properties, namely, hardness; toughness; stiffness; ductility; thermal, electrical, and magnetic properties; and microstructure effects on finishing methods. It also addresses the relative response of work materials, such as metals, ceramics, and composites, to grinding.

You do not currently have access to this chapter.
Don't already have an account? Register

K. Subramanian, Influence of Work Material Properties on Finishing Methods, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 161–164, https://doi.org/10.31399/asm.hb.v05.a0001241