Liquid Carburizing and Cyaniding of Steels[1]
-
Published:2013
Abstract
This article describes the uses of the liquid carburizing process carried out in low and high temperature cyanide-containing baths, and details the noncyanide liquid carburizing process which can be accomplished in a bath containing a special grade of carbon. It presents a simple formula for estimating total case depth, and illustrates the influence of carburizing temperature, duration of carburizing, quenching temperature, and quenching medium with the aid of typical hardness gradients. The article provides information on controlling of cyaniding time and temperature, bath composition, and case depth, and presents examples that relate dimensional change to several shapes that vary in complexity. It also provides information on the quenchant removal and salt removal processes, lists the applications of liquid carburizing in cyanide baths, and discusses the process and importance of cyanide waste disposal in detail.
Sign in
ASM members
Member Sign InJon Dossett, Liquid Carburizing and Cyaniding of Steels, Steel Heat Treating Fundamentals and Processes, Vol 4A, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2013, p 565–580, https://doi.org/10.31399/asm.hb.v04a.a0005778
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.