Skip to Main Content
Skip Nav Destination

Abstract

This article commences with a description of the principles of induction heating followed by a discussion on the high temperature electrical, magnetic, and thermal properties of steel, which influence the performance of induction heaters. The importance of eddy current distribution in a workpiece is explained, with emphasis on the skin effect. The article discusses typical procedures for induction hardening of steel, namely, austenitizing and quenching to form martensite either on the surface (case hardening) or through the entire section (through hardening). It briefly describes induction heating parameters for surface hardening, through hardening, tempering, and some general heating operations in metalworking.

You do not currently have access to this chapter.
Don't already have an account? Register

Valery Rudnev, Jon Dossett, Induction Surface Hardening of Steels, Steel Heat Treating Fundamentals and Processes, Vol 4A, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2013, p 438–461, https://doi.org/10.31399/asm.hb.v04a.a0005761

Download citation file:


Close
Close Modal

or Create an Account

Close Modal
Close Modal