Annealing of Steel[1]
-
Published:2013
Abstract
Steels may be annealed to facilitate cold working or machining, to improve mechanical or electrical properties, or to promote dimensional stability. This article, using iron-carbon phase diagram, describes the types of annealing processes, namely, subcritical annealing, intercritical annealing, supercritical or full annealing, and process annealing. Spheroidizing is performed for improving the cold formability of steels. The article provides guidelines for annealing and tabulates the critical temperature values for selected carbon and low-alloy steels and recommended temperatures and time cycles for annealing of alloy steels and carbon steel forgings. Different combinations of annealed microstructure and hardness are significant in terms of machinability. Furnaces for annealing are of two basic types, batch furnaces and continuous furnaces. The article concludes with a description of the annealing processes for steel sheets and strips, forgings, bars, rods, wires, and plates.
Sign in
ASM members
Member Sign InSatyam S. Sahay, Annealing of Steel, Steel Heat Treating Fundamentals and Processes, Vol 4A, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2013, p 289–304, https://doi.org/10.31399/asm.hb.v04a.a0005787
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.