Physical Properties of Carbon and Low-Alloy Steels[1]

Published:
1990
Page range:
195 - 199

Abstract

This article discusses the following physical properties of AISI and SAE grades of carbon and low-alloy steels: coefficients of linear thermal expansion; thermal conductivity; specific heat; and electrical resistivity.

You do not currently have access to this content.
Don't already have an account? Register

1990. "Physical Properties of Carbon and Low-Alloy Steels", Properties and Selection: Irons, Steels, and High-Performance Alloys, ASM Handbook Committee

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal