This article discusses tubular products made from wrought carbon or alloy constructional steels, particularly pipe, specialty tubing, and oil country tubular goods. The article covers product classifications, available specifications, chemical compositions, sizes, and other dimensional attributes. Some of the common types of pipe are standard pipe, conduit pipe, piling pipe, pipe for nipples, transmission or line pipe, water main and water well pipe, and pressure pipe. Pipe in suitable sizes and most products classified as tubing, both seamless and welded, may be cold finished. Pressure tubes, a separate classification, include double-wall brazed tubing, structural tubing, welded mechanical tubing, continuous-welded cold-finished mechanical tubing, and seamless mechanical tubing.

You do not currently have access to this chapter.
Don't already have an account? Register

Dennis Smyth, R.G. Lessard, Frank Minden, 1990. "Steel Tubular Products", Properties and Selection: Irons, Steels, and High-Performance Alloys, ASM Handbook Committee

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal