This article discusses the properties of threaded fasteners made from carbon and low-alloy steels containing a maximum of 0.55% carbon. It provides guidelines for the selection of steels for bolts, studs, and nuts intended for use at temperatures between -50 and 370 deg C. The article also discusses steels rated for service above 370 deg C and describes internationally recognized grade designations. The specifications provided can be used to outline fastener requirements, control manufacturing processes, and establish functional or performance standards. The most commonly used protective metal coatings for ferrous metal fasteners; zinc, cadmium, and aluminum; are described as well.

You do not currently have access to this chapter.
Don't already have an account? Register

ASM Committee on Threaded Steel Fasteners , Frank W. Akstens, James Gialamas, Edward J. Bueche, T.P. Madvad, Brian Murkey, Joseph McAuliffe, Gregory D. Sander, Edwin F. Frederick, Hal L. Miller, P.C. Hagopian, James Fox, 1990. "Threaded Steel Fasteners", Properties and Selection: Irons, Steels, and High-Performance Alloys, ASM Handbook Committee

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal