This article begins with an overview of steel wire configurations and sizes followed by a discussion on various wiremaking practices. The wiredrawing operation is discussed, including cleaning, die design, use of lubricants and welds, finishes, coating, and thermal treatments. Metallic coatings can be applied to wire by various methods, including hot dip processes, electrolytic process, and metal cladding by rolling metallic strip over the wire. These wires are normally grouped into broad usage categories. These categories, as well as some items in each category, are described in the article under their quality descriptions or commodity names. These include low-carbon steel wire for general usage, wire for structural applications, wire for packaging and container applications, wire for prestressed concrete, wire for electrical or conductor applications, rope wire, mechanical spring wire for general use, wire for fasteners, mechanical spring wire for special applications, upholstery spring construction wire, and alloy wire.

You do not currently have access to this chapter.
Don't already have an account? Register
Close Modal

or Create an Account

Close Modal
Close Modal