Abstract

Copper alloy castings are used in applications that require superior corrosion resistance, high thermal or electrical conductivity, good bearing surface qualities, or other special properties. This Article discusses the nominal composition and mechanical properties of copper casting alloys, designated in the Unified Numbering System. It also describes the selection factors of copper casting alloys, including castability, machinability, dimensional tolerances, bearing and wear properties, and cost considerations. The Article provides information on the relative corrosion resistance of 14 different classes of copper casting alloys in a wide variety of liquids and gases which helps in selecting alloys for corrosion service.

You do not currently have access to this chapter.
Don't already have an account? Register

Robert F. Schmidt, Donald G. Schmidt, 1990. "Selection and Application of Copper Alloy Castings", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal