Properties of Cast Aluminum Alloys

By
A.L. Kearney
A.L. Kearney
Revising author
Avery Kearney and Company
Search for other works by this author on:
Published:
1990
Page range:
152 - 177

Abstract

This Article is a compilation of property data for standard grades of cast aluminum alloys. Data are provided for mechanical, thermal, and electrical properties. The listing for each alloy includes commercial names, chemical compositions, applications, relevant specifications, fabrication characteristics, and mass characteristics.

You do not currently have access to this content.
Don't already have an account? Register

A.L. Kearney, 1990. "Properties of Cast Aluminum Alloys", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal