Skip to Main Content
ASM Handbook

Properties and Selection: Nonferrous Alloys and Special-Purpose Materials

By
ASM Handbook Committee
ASM Handbook Committee
Search for other works by this author on:
ASM International
Volume
2
ISBN electronic:
978-1-62708-162-7
Publication date:
1990
Book Chapter

Ordered Intermetallics

By
C.T. Liu
C.T. Liu
Metals and Ceramics Division, Oak Ridge National Laboratory
Search for other works by this author on:
;
J.O. Stiegler
J.O. Stiegler
Metals and Ceramics Division, Oak Ridge National Laboratory
Search for other works by this author on:
;
F.H. (Sam) Froes
F.H. (Sam) Froes
Institute for Materials and Advanced Processes, Colleges of Mines, University of Idaho
Search for other works by this author on:
Published:
1990
Page range:
913 - 942

Abstract

Ordered intermetallic compounds based on aluminides and silicides constitute a unique class of metallic materials that have promising physical and mechanical properties for structural applications at elevated temperatures. This Article provides useful information on mechanical and metallurgical properties, material processing and fabrication, structural applications, mechanical behavior, environmental embrittlement, alloying effects, and crystal structure of aluminides of nickel, iron, titanium, and silicides. It describes the cleavage and intergranular fracture in trialuminides.

You do not currently have access to this content.
Don't already have an account? Register

C.T. Liu, J.O. Stiegler, F.H. (Sam) Froes, 1990. "Ordered Intermetallics", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal