Skip to Main Content
ASM Handbook

Properties and Selection: Nonferrous Alloys and Special-Purpose Materials

By
ASM Handbook Committee
ASM Handbook Committee
Search for other works by this author on:
ASM International
Volume
2
ISBN electronic:
978-1-62708-162-7
Publication date:
1990
Book Chapter

Aluminum Foundry Products

By
A. Kearney
A. Kearney
Revising author
Avery Kearney & Company
Search for other works by this author on:
;
Elwin L. Rooy
Elwin L. Rooy
Revising author
Aluminum Company of America
Search for other works by this author on:
Published:
1990
Page range:
123 - 151

Abstract

Aluminum casting alloys are the most versatile of all common foundry alloys and generally have the highest castability ratings. This Article discusses the designation and classification of aluminum casting alloys based on their composition and the factors influencing alloy selection. Alloys discussed include rotor alloys, commercial duralumin alloys, premium casting alloys, piston and elevated-temperature alloys, general-purpose alloys, magnesium alloys, aluminum-zinc-magnesium alloys, and bearing alloys. Six basic types of aluminum alloys developed for casting include aluminum-copper, aluminum-copper-silicon, aluminum-silicon, aluminum-magnesium, aluminum-zinc-magnesium, and aluminum-tin. The Article also describes the main casting processes for aluminum alloys, which include die casting, permanent mold casting, sand casting (green sand and dry sand), plaster casting, and investment casting. In addition, the Article discusses factors affecting the mechanical and physical properties, microstructural features that affect mechanical properties, the effects of alloying, and major applications of aluminum casting alloys.

You do not currently have access to this content.
Don't already have an account? Register

A. Kearney, Elwin L. Rooy, 1990. "Aluminum Foundry Products", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal