Wrought Copper and Copper Alloy Products

By
Derek E. Tyler
Derek E. Tyler
Revising author
Olin Corporation
Search for other works by this author on:
Published:
1990
Page range:
241 - 264

Abstract

Wrought copper and copper alloys are produced in various mill-product forms for a variety of applications due to their high electrical conductivity, corrosion resistance, ease of fabrication, and good heat-transfer properties. This Article describes the manufacturing processes used to produce wrought copper and copper alloys in the form of sheet and strip products, tubular products, and wire and cable. Common processes include melting, casting, hot and cold rolling, milling or scalping, annealing, cleaning, slitting, cutting, and leveling. In addition, the Article discusses stress-relaxation characteristics of copper alloys.

You do not currently have access to this content.
Don't already have an account? Register

Derek E. Tyler, 1990. "Wrought Copper and Copper Alloy Products", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal