Abstract

Ternary molybdenum chalcogenides stands for a vast class of materials, whose general formula is MxMO6X8, where, M is a cation and X is a chalcogen (sulfur, selenium, or tellurium). Possible applications of some of these are as high field superconductors (that is, >20 T, or 200 kG). This Article discusses the fabrication methods of PbMo6S8 (PMS) and SnMo6S8 (SMS), including hot processing and cold processing. It provides a short note on the superconducting properties of PMS wire filaments and their applications in processes requiring high magnetic fields, such as high-energy physics, thermonuclear fusion, and nuclear magnetic resonance.

You do not currently have access to this chapter.
Don't already have an account? Register

Luc Le Lay, 1990. "Ternary Molybdenum Chalcogenides (Chevrel Phases)", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal