Skip to Main Content
ASM Handbook

Properties and Selection: Nonferrous Alloys and Special-Purpose Materials

By
ASM Handbook Committee
ASM Handbook Committee
Search for other works by this author on:
ASM International
Volume
2
ISBN electronic:
978-1-62708-162-7
Publication date:
1990
Book Chapter

Indium and Bismuth

By
Laurence G. Stevens
Laurence G. Stevens
Indium Corporation of America
Search for other works by this author on:
;
C.E.T. White
C.E.T. White
Indium Corporation of America
Search for other works by this author on:
Published:
1990
Page range:
750 - 757

Abstract

Indium and bismuth, although distinct in several properties and areas of application, have relatively low melting temperatures and some common areas of application. This Article discusses two significant uses of indium and bismuth alloys, namely, in low-melting-temperature solders and in fusible alloys. It provides a brief note on the occurrence, recovery and production processes, and several other areas of application. Tables provide helpful information on the designation, classification, composition, properties, suitability, and temperatures ranges of these alloys.

You do not currently have access to this content.
Don't already have an account? Register

Laurence G. Stevens, C.E.T. White, 1990. "Indium and Bismuth", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal