Tin and Tin Alloys

By
William B. Hampshire
William B. Hampshire
Revising author
Tin Research Institute, Inc.
Search for other works by this author on:
Published:
1990
Page range:
517 - 526

Abstract

Tin is produced from both primary and secondary sources. This Article discusses the chemical compositions, production, properties, microstructure and applications of tin and tin alloys. The major tin alloys discussed here are tin-antimony-copper alloy (pewter), bearing alloy, solder alloy and other alloys containing traces of tin. Data on tin consumption in the United States is presented graphically.

You do not currently have access to this content.
Don't already have an account? Register

William B. Hampshire, 1990. "Tin and Tin Alloys", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee