Properties of Magnesium Alloys

By
Susan Housh
Susan Housh
Revising author
Dow Chemical U.S.A.
Search for other works by this author on:
;
Barry Mikucki
Barry Mikucki
Revising author
Dow Chemical U.S.A.
Search for other works by this author on:
;
Archie Stevenson
Archie Stevenson
Revising author
Magnesium Elektron, Inc.
Search for other works by this author on:
Published:
1990
Page range:
480 - 516

Abstract

This Article is a compilation of property data for standard grades of wrought magnesium and cast magnesium alloys. Data are provided for mechanical, physical, thermal, and electrical properties. Valuable information is provided regarding the applications, chemical compositions, relevant specifications, fabrication characteristics and mass characteristics of each alloy.

You do not currently have access to this content.
Don't already have an account? Register

Susan Housh, Barry Mikucki, Archie Stevenson, 1990. "Properties of Magnesium Alloys", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee