Aluminum-Lithium Alloys

By
Richard S. James
Richard S. James
Aluminum Company of America
Search for other works by this author on:
Published:
1990
Page range:
178 - 199

Abstract

Aluminum-lithium alloys have been developed primarily to reduce the weight of aircraft and aerospace structures. This Article commences with a discussion on the physical metallurgy and development of aluminum-lithium alloys. It focuses on major commercial aluminum-lithium alloys, including alloy 2090, alloy 2091, alloy 8090, alloy CP276, and Weldalite 049. The Article also lists the chemical compositions, physical properties, fabrication characteristics, corrosion performance, and general applications of these alloys. A comparison of alloy properties is represented graphically.

You do not currently have access to this content.
Don't already have an account? Register

Richard S. James, 1990. "Aluminum-Lithium Alloys", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee