Properties of Cast Aluminum Alloys
By
A.L. Kearney
A.L. Kearney
Revising author
Avery Kearney and Company
Search for other works by this author on:
-
Published:1990
Abstract
This Article is a compilation of property data for standard grades of cast aluminum alloys. Data are provided for mechanical, thermal, and electrical properties. The listing for each alloy includes commercial names, chemical compositions, applications, relevant specifications, fabrication characteristics, and mass characteristics.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
A.L. Kearney, Properties of Cast Aluminum Alloys, Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, Vol 2, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 152–177, https://doi.org/10.31399/asm.hb.v02.a0001062
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Book Content
Properties of Magnesium Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Properties of Precious Metals
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Properties of Wrought Aluminum and Aluminum Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Properties of Wrought Coppers and Copper Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Properties of Pure Metals
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Temperature Requirements for Heating Titanium, Aluminum, Magnesium, and Copper Alloys
Induction Heating and Heat Treatment
Properties of Cast Copper Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Tin and Tin Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Steel Bar, Rod, and Wire
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Engineering Tables: Reinforcement Materials
Engineered Materials Handbook Desk Edition