Abstract
This Article is a compilation of the property data for standard grades of wrought copper and copper alloys. Data are provided for mechanical, physical, thermal, electrical, optical, and magnetic properties. The list for each alloy includes its commercial names, chemical composition, relevant specifications and standards, fabrication characteristics, mass characteristics, and applications.
Sign in
ASM members
Member Sign InPeter Robinson, Properties of Wrought Coppers and Copper Alloys, Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, Vol 2, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 265–345, https://doi.org/10.31399/asm.hb.v02.a0001067
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.