Properties of Wrought Aluminum and Aluminum Alloys
-
Published:1990
Abstract
This article discusses the chemical composition, mechanical, physical, thermal, electrical, optical, and magnetic properties of a variety of grades of wrought aluminum and aluminum alloys. It also discusses the standard specifications, mass and fabrication characteristics, corrosion resistance, and applications of a variety of grades of wrought aluminum and aluminum alloys.
Sign in
ASM members
Member Sign InProperties of Wrought Aluminum and Aluminum Alloys, Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, Vol 2, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 62–122, https://doi.org/10.31399/asm.hb.v02.a0001060