Abstract

Niobium-titanium alloys (NbTi) became the superconductors of choice in the early 1960s, providing a viable alternative to the A-15 compounds and less ductile alloys of niobium-zirconium. This can be attributed to the relative ease of fabrication, better electrical properties, and greater compatibility with copper stabilizing materials. This Article discusses the ramifications of design requirements, selection criteria and processing methods of superconducting fibers and matrix materials. It provides information on the various steps involved in the fabrication of superconducting composites, including assembly, welding, isostatic compaction, extrusion, wire drawing, twisting, and final sizing. The Article also provides a detailed account of the properties and applications of NbTi superconducting composites.

You do not currently have access to this chapter.
Don't already have an account? Register

T. Scott Kreilick, Niobium-Titanium Superconductors, Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, Vol 2, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 1043–1059, https://doi.org/10.31399/asm.hb.v02.a0001110

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal