Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Properties of Cast Copper Alloys
-
Published:1990
Abstract
This Article is a compilation of property data for standard grades of cast copper alloys. Data are provided for mechanical, physical, thermal, electrical, chemical, nuclear, optical, and magnetic properties. The list for each alloy includes its common name, chemical composition, applications, mass characteristics, and fabrication characteristics.
Sign in
ASM members
Member Sign InArthur Cohen, Properties of Cast Copper Alloys, Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, Vol 2, ASM Handbook, By ASM Handbook Committee, ASM International, 1990, p 356–391, https://doi.org/10.31399/asm.hb.v02.a0001069