Abstract

This appendix provides fracture toughness and tensile property data for aluminum alloys in the 2000, 6000, 7000, and 8000 series as well as B201 and D357 aluminum castings and powder metal alloys.

You do not currently have access to this chapter.
Don't already have an account? Register

Mechanical Properties Data for Selected Aluminum Alloys, Mechanics and Mechanisms of Fracture: An Introduction, By Alan F. Liu, ASM International, 2005, p 397–409, https://doi.org/10.31399/asm.tb.mmfi.t69540397