This chapter discusses the phase transformations of peritectic alloy systems. It describes the processes involved with equilibrium and nonequilibrium freezing, the mechanisms of peritectic formation, and the resulting microstructures. It also discusses the formation of peritectic structures in iron-base alloys and multicomponent systems.

You do not currently have access to this chapter.
Don't already have an account? Register

Peritectic Alloy Systems, Phase Diagrams: Understanding the Basics, Edited By F.C. Campbell, ASM International, 2012, p 117–134, https://doi.org/10.31399/asm.tb.pdub.t53420117