The process of transferring coating materials from the container to the surface to be coated can be accomplished in a number of ways. This article describes seven methods of coating application: brushes, rollers, and daubers; conventional air spray; high-volume low-pressure spray; airless spray; air-assisted airless spray; plural-component spray; and electrostatic spray. Factors to be considered when deciding on an application method include the size and configuration of the surfaces to be coated, the type of coating being applied, environmental regulations/restrictions, the proximity to other operations or personnel, and the recommendations of the coating manufacturer.