Skip to Main Content
ASM Handbook

Protective Organic Coatings

Edited by
Kenneth B. Tator
Kenneth B. Tator
KTA-Tator, Inc.
Search for other works by this author on:
ASM International
Volume
5B
ISBN electronic:
978-1-62708-172-6
Publication date:
2015
Book Chapter

Guidelines for Maintenance Coating of Steel Structures in Pulp and Paper Mills

By
R.A. Nixon
R.A. Nixon
Corrosion Probe, Inc.
Search for other works by this author on:
;
D. Bennett
D. Bennett
Corrosion Probe, Inc.
Search for other works by this author on:
Published:
2015
Page range:
422 - 437

Abstract

Maintenance coating is an important part of any meaningful asset-preservation strategy in facilities producing pulp and paper and other chemicals. This article discusses maintenance coating for carbon steel structures and process equipment exposed to normal external pulp and paper mill atmospheric conditions. The important requirements and standards for surface preparation are emphasized and common issues encountered in maintenance coating projects are described.

You do not currently have access to this content.
Don't already have an account? Register

R.A. Nixon, D. Bennett, 2015. "Guidelines for Maintenance Coating of Steel Structures in Pulp and Paper Mills", Protective Organic Coatings, Kenneth B. Tator

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal