Powder coatings are widely used by manufacturers as a finish of choice to enhance the appearance and performance of their products. This article begins with a discussion on advantages and disadvantages of powder coatings. It describes the selection of coating-types and uses of powder coatings in appliance industries, furniture industries, computer industries, fixture industries, architectural industries, automotive industries, agriculture and construction equipment industries, recreational equipment industries, and general industries. Powder coating formulations consist of binder systems, pigments, extenders, and additives. The basic process flow for the manufacture of powder coatings consists of premix, extrusion, grinding, and packing. The article...