Abstract
Two-component polyurea elastomeric coating/lining systems are the newest technology in the protective coating/lining industry and a wide variety of applications have been developed. These include coating/lining applications over concrete, geotextile membranes, various metals for corrosion and decorative areas, and some plastics. This article discusses the formulation basics of polyurea technology and compares the technology to that of polyurethane and polyurethane/polyurea systems. It addresses performance issues and describes application processing considerations and safety practices of polyurea coating/lining systems.
Sign in
ASM members
Member Sign InDudley J. Primeaux, II, Polyurea-Based Coatings, Protective Organic Coatings, Vol 5B, ASM Handbook, Edited By Kenneth B. Tator, ASM International, 2015, p 118–131, https://doi.org/10.31399/asm.hb.v05b.a0006047
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.