Managing corrosion continues to be a challenge for operators of modern boilers worldwide. This chapter addresses the corrosion-related problems that can occur in boilers burning municipal solid waste (MSW). It describes corrosion mechanisms associated with different environments and alloys. It also discusses corrosion protection methods for furnace waterwalls and superheater tubes in waste-to-energy boilers.

You do not currently have access to this chapter.
Don't already have an account? Register

Waste-to-Energy Boilers and Waste Incinerators, High-Temperature Corrosion and Materials Applications, By George Y. Lai, ASM International, 2007, p 335–358, https://doi.org/10.31399/asm.tb.htcma.t52080335